| MOQ: | 1 Piece/Pieces |
| Delivery Period: | 4-8weeks |
| Payment Method: | T/T |
| Supply Capacity: | 100,000/year |
445nm-50W
Features:
445nm wavelength
50W output power
113µm fiber core diameter
0.15NA
BPP=8 mm. mrad
Applications:
Material Processing
| Specifications(20℃) | Symbol | Unit | K445HR7FN-50.00WN1N-11315 | |||
| Minimum | Typical | Maximum | ||||
| Optical Data(1) | Total CW Output Power | Pbol (4) | W | 50 | - | - |
| Number of submodules | pcs | - | - | 2 | - | |
| Submodule CW Output Power | Po | W | - | 25 | - | |
| Center Wavelength | lc | nm | 445±20 | |||
| Spectral Width (FWHM) | △l | nm | - | 6 | - | |
| Wavelength Shift with Temperature | △l/△T | nm/℃ | - | 0.1 | - | |
| Wavelength Shift with Current | △l/△A | nm/A | - | 1 | - | |
| Electrical Data | Electrical-to-Optical Efficiency | PE | % | - | 30 | - |
| Operating Current | Ibol (4) | A | - | 2.5 | 3.5 | |
| Threshold Current | Ith | A | - | 0.35 | - | |
| Operating Voltage(single module) | Vop | V | - | 35 | 40 | |
| Slope Efficiency(single module) | η | W/A | - | 11.5 | - | |
| Power Supply Mode | - | - | - | 2 modules | - | |
| Fiber Data | Core Diameter | Dcore | µm | - | 113 | - |
| Numerical Aperture | NA | - | - | 0.15 | - | |
| Minimum Bending Radius | - | mm | 50 | - | - | |
| Fiber Termination | - | - | - | SMA905 | - | |
| Thermistor | - | Rt | (KΩ)/β(25℃) | - | 10±3%/3450 | - |
| Others | ESD | Vesd | V | - | - | 500 |
| Storage Temperature (2) | Tst | ℃ | -20 | 70 | ||
| Lead Soldering Temp | Tls | ℃ | - | - | 260 | |
| Lead Soldering Time | t | sec | - | - | 10 | |
| Operating Temperature (3) | Top | ℃ | 15 | - | 30 | |
| Relative Humidity | RH | % | 15 | - | 75 | |
| MOQ: | 1 Piece/Pieces |
| Delivery Period: | 4-8weeks |
| Payment Method: | T/T |
| Supply Capacity: | 100,000/year |
445nm-50W
Features:
445nm wavelength
50W output power
113µm fiber core diameter
0.15NA
BPP=8 mm. mrad
Applications:
Material Processing
| Specifications(20℃) | Symbol | Unit | K445HR7FN-50.00WN1N-11315 | |||
| Minimum | Typical | Maximum | ||||
| Optical Data(1) | Total CW Output Power | Pbol (4) | W | 50 | - | - |
| Number of submodules | pcs | - | - | 2 | - | |
| Submodule CW Output Power | Po | W | - | 25 | - | |
| Center Wavelength | lc | nm | 445±20 | |||
| Spectral Width (FWHM) | △l | nm | - | 6 | - | |
| Wavelength Shift with Temperature | △l/△T | nm/℃ | - | 0.1 | - | |
| Wavelength Shift with Current | △l/△A | nm/A | - | 1 | - | |
| Electrical Data | Electrical-to-Optical Efficiency | PE | % | - | 30 | - |
| Operating Current | Ibol (4) | A | - | 2.5 | 3.5 | |
| Threshold Current | Ith | A | - | 0.35 | - | |
| Operating Voltage(single module) | Vop | V | - | 35 | 40 | |
| Slope Efficiency(single module) | η | W/A | - | 11.5 | - | |
| Power Supply Mode | - | - | - | 2 modules | - | |
| Fiber Data | Core Diameter | Dcore | µm | - | 113 | - |
| Numerical Aperture | NA | - | - | 0.15 | - | |
| Minimum Bending Radius | - | mm | 50 | - | - | |
| Fiber Termination | - | - | - | SMA905 | - | |
| Thermistor | - | Rt | (KΩ)/β(25℃) | - | 10±3%/3450 | - |
| Others | ESD | Vesd | V | - | - | 500 |
| Storage Temperature (2) | Tst | ℃ | -20 | 70 | ||
| Lead Soldering Temp | Tls | ℃ | - | - | 260 | |
| Lead Soldering Time | t | sec | - | - | 10 | |
| Operating Temperature (3) | Top | ℃ | 15 | - | 30 | |
| Relative Humidity | RH | % | 15 | - | 75 | |